PEROXAN PMB-Paste 50 SI is recommended for crosslinking of silicone rubber.
When crosslinked with PEROXAN PMBP-Paste 50 SI, the peroxide decomposes into chlorine-free decomposition products, means no polychlorinated biphenyls (PCB) are generated.
With PEROXAN PMB-Paste 50 SI silicone rubber compounds can be cured without external pressure (hot air and/or IR vulcanization).
PEROXAN PMB-Paste 50 Si can be incorporated easily into a silicone rubber compound on a 2-roll mill.
Dosing (silicone rubber): 1 to 2 phr
Safe processing temperature (t2): 80°C
Typical crosslinking temperature (t90): 110°C
The safe processing temperature t2 is defined as the temperature, at which the scorch time is longer than 20 minutes.
The typical crosslinking temperature t90 is defined as the temperature at which 90% of the crosslinks in the compound are formed within about 12 minutes.