Polymerization of ethylene:
PEROXAN PK234 W is used for high pressure polymerization of ethylene in both autoclave and tubular processes, usually in combination with other peroxides of varying degrees of activity.
Temperature range: 190 to 250°C
Light-off temperature at 2300 bar: 219°C
Polymerization of styrene:
PEROXAN PK234 W may be used in polymerization and copolymarization of styrene.
In a mass process PEROXAN PK234 W can be used to increase polymerization rates.
In suspension polymerization processes, PEROXAN PK234 W is often used for reduction of residual styrene content during the final polymerization stage.
Temperature range: 90 to 130°C
Dosing: 0,02 to 0,1 phr
Polymerization of acrylates and methacrylates:
PEROXAN PK234 W can be used as initiator for the solution, bulk and suspension (co)polymerization of acrylates and methacrylates.
Temperature range: 100 to 140°C
Dosing: 0,1 to 1 phr
Other applications:
PEROXAN PK234 W may also be used for the (co)polymerization of acrylonitrile and divinylbenzene.